09

2025-07

Key Factors Influencing the Melting Rate in Glass Furnaces

The melting rate refers to the ratio of daily output to the furnace‘s melting area. However, since the melting rate involves multiple factors, a more reasonable and comprehensive indicator is theperiodic melting rate. When selecting the melting rate for furnace desig··· ...

09

2025-07

Measures to Extend the Service Life of Glass Furnaces

Glass furnaces have a defined operational cycle. The design lifespan is one factor, but if production output and quality significantly decline over time while costs rise, the furnace should enter a cold repair phase. In recent years, with advancements in refractory ma··· ...

08

2025-07

Talking about how to reduce the explosion of sidewall blocks in the baking glass furnace

The life of the sidewall blocks in the float glass furnace is one of the important factors that determine the life of the glass furnace. However, the use of fused cast AZS blocks on the side wall is very easy to produce cracks when baking the glass furnace, which seri··· ...

08

2025-07

What factors affect the resistance of fused cast AZS blocks in glass furnaces to erosion by glass liquid?

Glass furnaces are the core equipment in the glass industry. Their service life and the quality of glass products directly depend on the anti-erosion performance of refractory materials.Fused cast AZS blocks, due to their excellent high-temperature stability, chemical··· ...

07

2025-07

Fused Cast AZS Arch Blocks:

Fused cast AZS arch blocks mainly play a role in supporting the structure, enhancing stability and load-bearing capacity, and they are also a key part of the flame space, playing an important role in the radiation and heat transfer of the flame.1.High refractorinessFu··· ...

07

2025-07

Discussion on hot replacement of tuck stones at port neck in glass furnace production

The glass furnace is the heart of a glass factory, and its operational safety is extremely important. As a large-scale thermal complex, the maximum flame temperature in the operation space of a furnace is generally above 1600℃, and the maximum temperature of the glas··· ...

30

2025-06

Selection and Application of Fused Cast AZS Blocks for Oxy-fuel Combustion Glass Furnace

Selection and Application of Fused Cast AZS Blocks for Oxy-fuel Combustion Glass FurnaceAll-oxygen combustion technology is a combustion mode that uses "oxygen + fuel" instead of "air + fuel". Adopting all-oxygen combustion technology can achieve e··· ...

30

2025-06

Causes of cracks in silica bricks

Silica bricks are prone to various cracks during the production process, such as spalling, vertical cracks, transverse cracks and network cracks. The rejection rate of silica bricks is high, and its yield rate is not as high as other refractory bricks. Please see the ··· ...

13

2025-06

Detailed explanation of AZS bricks (zirconia corundum bricks) technology for glass kilns

1. Introduction to AZS bricksAZS bricks (Alumina-Zirconia-Silica, i.e. alumina-zirconia-silica refractory materials) are the core refractory materials for key parts of glass kilns (such as melting pools, flow holes, and kiln sills). They are widely used due to their e··· ...

13

2025-06

Detailed explanation of AZS bricks (zirconia corundum bricks) technology for glass kilns

1. Introduction to AZS bricksAZS bricks (Alumina-Zirconia-Silica, i.e. alumina-zirconia-silica refractory materials) are the core refractory materials for key parts of glass kilns (such as melting pools, flow holes, and kiln sills). They are widely used due to their e··· ...